Skip to Main Content
ASM Handbook

Casting

Edited by
Srinath Viswanathan
Srinath Viswanathan
Search for other works by this author on:
Diran Apelian
Diran Apelian
Search for other works by this author on:
Raymond J. Donahue
Raymond J. Donahue
Search for other works by this author on:
Babu DasGupta
Babu DasGupta
Search for other works by this author on:
Michael Gywn
Michael Gywn
Search for other works by this author on:
John L. Jorstad
John L. Jorstad
Search for other works by this author on:
Raymond W. Monroe
Raymond W. Monroe
Search for other works by this author on:
Mahi Sahoo
Mahi Sahoo
Search for other works by this author on:
Thomas E. Prucha
Thomas E. Prucha
Search for other works by this author on:
Daniel Twarog
Daniel Twarog
Search for other works by this author on:
ASM International
Volume
15
ISBN electronic:
978-1-62708-187-0
Publication date:
2008
Book Chapter

Crucible Furnaces

By
George Giles
George Giles
Morgan Molten Metal Systems
Search for other works by this author on:
Published:
2008
Page range:
155 - 159
Publication history
September 05, 2008

Abstract

This article discusses the design parameters, operation, characteristics, properties, and advantages of various types of crucible furnaces, such as stationary, tilting, and movable furnaces. It also provides information on the application of the crucible furnaces.

You do not currently have access to this content.
Don't already have an account? Register

George Giles, 2008. "Crucible Furnaces", Casting, Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal