Skip to Main Content
ASM Handbook

Casting

Edited by
Srinath Viswanathan
Srinath Viswanathan
Search for other works by this author on:
Diran Apelian
Diran Apelian
Search for other works by this author on:
Raymond J. Donahue
Raymond J. Donahue
Search for other works by this author on:
Babu DasGupta
Babu DasGupta
Search for other works by this author on:
Michael Gywn
Michael Gywn
Search for other works by this author on:
John L. Jorstad
John L. Jorstad
Search for other works by this author on:
Raymond W. Monroe
Raymond W. Monroe
Search for other works by this author on:
Mahi Sahoo
Mahi Sahoo
Search for other works by this author on:
Thomas E. Prucha
Thomas E. Prucha
Search for other works by this author on:
Daniel Twarog
Daniel Twarog
Search for other works by this author on:
ASM International
Volume
15
ISBN electronic:
978-1-62708-187-0
Publication date:
2008
Book Chapter

Automation in High-Pressure Die Casting

By
Yeou-Li Chu
Yeou-Li Chu
Ryobi Die Casting
Search for other works by this author on:
Published:
2008
Page range:
747 - 758
Publication history
September 15, 2008

Abstract

High-pressure die casting is a fast method for net shape manufacturing of parts from nonferrous alloys. This article reviews the automation technologies for the different stages or steps of the process. The steps include liquid metal pouring, injection, solidification, die open, part extraction, die lubrication, insert loading, and die close. Some manual aspects of the operations together with automation options are discussed. The article describes finishing steps, such as finish trimming, detailed deflashing, shot blast cleaning, and quality checks. Automation of the postcasting process is also discussed.

You do not currently have access to this content.
Don't already have an account? Register

Yeou-Li Chu, 2008. "Automation in High-Pressure Die Casting", Casting, Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal