Skip to Main Content
ASM Handbook

Casting

Edited by
Srinath Viswanathan
Srinath Viswanathan
Search for other works by this author on:
Diran Apelian
Diran Apelian
Search for other works by this author on:
Raymond J. Donahue
Raymond J. Donahue
Search for other works by this author on:
Babu DasGupta
Babu DasGupta
Search for other works by this author on:
Michael Gywn
Michael Gywn
Search for other works by this author on:
John L. Jorstad
John L. Jorstad
Search for other works by this author on:
Raymond W. Monroe
Raymond W. Monroe
Search for other works by this author on:
Mahi Sahoo
Mahi Sahoo
Search for other works by this author on:
Thomas E. Prucha
Thomas E. Prucha
Search for other works by this author on:
Daniel Twarog
Daniel Twarog
Search for other works by this author on:
ASM International
Volume
15
ISBN electronic:
978-1-62708-187-0
Publication date:
2008
Book Chapter

Approaches to Measurement of Metal Quality[1]

By
Rathindra DasGupta
Rathindra DasGupta
National Science Foundation
Search for other works by this author on:
Published:
2008
Page range:
1167 - 1173
Publication history
October 14, 2008

Abstract

Several qualitative, semiquantitative, and quantitative tests are available to estimate and control metal cleanliness, particularly inclusion concentration of aluminum alloys. This article provides a brief description of few of the metal cleanliness assessment techniques, such as chemical analysis, pressure filter tests, electric resistivity tests, reduced-pressure test, and ultrasonic technique. It also lists the various impurities detection methods of chemical analysis and their limitations.

You do not currently have access to this content.
Don't already have an account? Register

Rathindra DasGupta, 2008. "Approaches to Measurement of Metal Quality", Casting, Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal