Skip to Main Content
ASM Handbook

Casting

Edited by
Srinath Viswanathan
Srinath Viswanathan
Search for other works by this author on:
Diran Apelian
Diran Apelian
Search for other works by this author on:
Raymond J. Donahue
Raymond J. Donahue
Search for other works by this author on:
Babu DasGupta
Babu DasGupta
Search for other works by this author on:
Michael Gywn
Michael Gywn
Search for other works by this author on:
John L. Jorstad
John L. Jorstad
Search for other works by this author on:
Raymond W. Monroe
Raymond W. Monroe
Search for other works by this author on:
Mahi Sahoo
Mahi Sahoo
Search for other works by this author on:
Thomas E. Prucha
Thomas E. Prucha
Search for other works by this author on:
Daniel Twarog
Daniel Twarog
Search for other works by this author on:
ASM International
Volume
15
ISBN electronic:
978-1-62708-187-0
Publication date:
2008
Book Chapter

Steel Continuous Casting

By
Robert D. Pehlke
Robert D. Pehlke
University of Michigan
Search for other works by this author on:
Published:
2008
Page range:
918 - 925
Publication history
September 04, 2008

Abstract

This article outlines the advantages of the steel continuous casting, along with its developments and challenges for improvement. It describes the process of the steel continuous casting. The article provides a description of the design and layout of a steelmaking facility for continuous casting of steel. It reviews the trends in the steel industry, such as near-net shape casting, the use of tundish metallurgy, and pouring stream protection. The article discusses the use and capabilities of different molds for steel continuous casting. These include thin-wall tube-type molds, solid molds, and plate molds. The article explains the operations for productivity improvements and quality improvements in steel continuous casting. It reviews the applications of horizontal continuous casting in casting steel. An emphasis on the development of continuous casting depending on control systems and automation, with the objective of maintaining high quality and high productivity, is also provided.

You do not currently have access to this content.
Don't already have an account? Register

Robert D. Pehlke, 2008. "Steel Continuous Casting", Casting, Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal