Skip to Main Content
ASM Handbook

Casting

Edited by
Srinath Viswanathan
Srinath Viswanathan
Search for other works by this author on:
Diran Apelian
Diran Apelian
Search for other works by this author on:
Raymond J. Donahue
Raymond J. Donahue
Search for other works by this author on:
Babu DasGupta
Babu DasGupta
Search for other works by this author on:
Michael Gywn
Michael Gywn
Search for other works by this author on:
John L. Jorstad
John L. Jorstad
Search for other works by this author on:
Raymond W. Monroe
Raymond W. Monroe
Search for other works by this author on:
Mahi Sahoo
Mahi Sahoo
Search for other works by this author on:
Thomas E. Prucha
Thomas E. Prucha
Search for other works by this author on:
Daniel Twarog
Daniel Twarog
Search for other works by this author on:
ASM International
Volume
15
ISBN electronic:
978-1-62708-187-0
Publication date:
2008
Book Chapter

Ductile Iron Castings[1]

By
George M. Goodrich
George M. Goodrich
Stork Climax Research Services
Search for other works by this author on:
Published:
2008
Page range:
856 - 871
Publication history
October 14, 2008

Abstract

This article begins with a description of the classes and grades of ductile iron. It discusses the factors affecting the mechanical properties of ductile iron. The article reviews the hardness properties, tensile properties, shear and torsional properties, compressive properties, fatigue properties, fracture toughness, and physical properties of ductile iron and compares them with other cast irons to aid the designer in materials selection. It concludes with information on austempered ductile iron.

You do not currently have access to this content.
Don't already have an account? Register

George M. Goodrich, 2008. "Ductile Iron Castings", Casting, Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal