Skip to Main Content
ASM Handbook

Casting

Edited by
Srinath Viswanathan
Srinath Viswanathan
Search for other works by this author on:
Diran Apelian
Diran Apelian
Search for other works by this author on:
Raymond J. Donahue
Raymond J. Donahue
Search for other works by this author on:
Babu DasGupta
Babu DasGupta
Search for other works by this author on:
Michael Gywn
Michael Gywn
Search for other works by this author on:
John L. Jorstad
John L. Jorstad
Search for other works by this author on:
Raymond W. Monroe
Raymond W. Monroe
Search for other works by this author on:
Mahi Sahoo
Mahi Sahoo
Search for other works by this author on:
Thomas E. Prucha
Thomas E. Prucha
Search for other works by this author on:
Daniel Twarog
Daniel Twarog
Search for other works by this author on:
ASM International
Volume
15
ISBN electronic:
978-1-62708-187-0
Publication date:
2008
Book Chapter

Semisolid Casting—Introduction and Fundamentals

By
Q.Y. Pan
Q.Y. Pan
SPX Corporation
Search for other works by this author on:
Diran Apelian
Diran Apelian
Worcester Polytechnic Institute
Search for other works by this author on:
John Jorstad
John Jorstad
J.L.J. Technologies, Inc.
Search for other works by this author on:
Published:
2008
Page range:
761 - 763
Publication history
December 06, 2008

Abstract

Semisolid metal (SSM) processing, also known as semisolid metal casting, semisolid forming, or semisolid metal forging, is a special die casting process. This article discusses the origin and advantages of the SSM processing. It describes three major semisolid processing routes: thixocasting, rheocasting, and thixomolding.

You do not currently have access to this content.
Don't already have an account? Register

Q.Y. Pan, Diran Apelian, John Jorstad, 2008. "Semisolid Casting—Introduction and Fundamentals", Casting, Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog