Skip to Main Content
ASM Handbook

Corrosion: Environments and Industries

Edited by
Stephen D. Cramer
Stephen D. Cramer
Search for other works by this author on:
Bernard S. Covino, Jr.
Bernard S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13C
ISBN electronic:
978-1-62708-184-9
Publication date:
2006
Book Chapter

Corrosion in Petroleum Production Operations

By
Russell D. Kane
Russell D. Kane
Revising author
Honeywell Process Solutions, Honeywell International, Inc.
Search for other works by this author on:
Published:
2006
Page range:
922 - 966
Publication history
October 10, 2006

Abstract

This article discusses the particular corrosion problems encountered and the corrosion control methods used in petroleum production (i.e.,upstream) and the storage and transportation of oil and gas (i.e., midstream) up to the refinery (i.e., downstream). These control methods include proper material selection, protective coatings, cathodic protection systems, use of inhibitors, use of nonmetallic materials, and control of the environment. The article reviews the aspects of corrosion that tend to be unique to corrosion as encountered in applications involving oil and gas exploration and production. It discusses corrosion problems that are specific to the various types of environments or equipment used in secondary recovery, including producing wells, producing flow lines, and injection wells. Corrosion mitigation methods and guidelines are also discussed for each type of environment.

You do not currently have access to this content.
Don't already have an account? Register

Russell D. Kane, 2006. "Corrosion in Petroleum Production Operations", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal