Skip to Main Content
ASM Handbook

Corrosion: Environments and Industries

Edited by
Stephen D. Cramer
Stephen D. Cramer
Search for other works by this author on:
Bernard S. Covino, Jr.
Bernard S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13C
ISBN electronic:
978-1-62708-184-9
Publication date:
2006
Book Chapter

Corrosion in Petroleum Refining and Petrochemical Operations

By
Russell D. Kane
Russell D. Kane
Revising author
Honeywell Process Solutions, Honeywell International, Inc.
Search for other works by this author on:
Published:
2006
Page range:
967 - 1014
Publication history
October 11, 2006

Abstract

This article presents the primary considerations and mechanisms for corrosion and explains how they are involved in the selection of materials for process equipment in refineries and petrochemical plants. It discusses the material selection criteria for a number of ferrous and nonferrous alloys used in petroleum refining and petrochemical applications. The article reviews the mechanical properties, fabricability, and corrosion resistance of refinery steels. It describes low- and high-temperature corrosion, hydrogen embrittlement, and cracking such as stress-corrosion, sulfide stress, and stress-oriented hydrogen-induced cracking. The article considers hydrogen attack, corrosion fatigue, and liquid metal embrittlement and the methods of combating them. It explains the causes of velocity-accelerated corrosion and erosion-corrosion. The article summarizes some corrective measures that can be implemented to control corrosion. The applicable standards for materials used in corrosive service conditions in upstream and downstream petroleum service are presented in a tabular form.

You do not currently have access to this content.
Don't already have an account? Register

Russell D. Kane, 2006. "Corrosion in Petroleum Refining and Petrochemical Operations", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.