Corrosion in the Pulp and Paper Industry[1]

By
Harry Dykstra
Harry Dykstra
Acuren
Search for other works by this author on:
Published:
2006
Page range:
762 - 802
Publication history
October 12, 2006

Abstract

This article discusses the methods of pulp production, pulp processing, pulp bleaching, and paper manufacturing. It describes various types of digesters, their construction materials, the corrosion problems encountered, and methods to protect these digesters from corrosion. The article examines the corrosion problems in high-yield mechanical pulping, sulfite process, neutral sulfite semichemical pulping, chemical recovery, tall oil plants, wastewater treatment, and recovery boilers. It explains the stages of chlorine-based and nonchlorine bleaching, process water reuse for elemental chlorine-free and nonchlorine bleaching stages, selection of material for bleaching equipment, developments in oxygen bleaching, and the use of highly corrosion-resistant materials for bleach plant equipment. The article reviews the materials used in the construction of paper machine components and specific corrosion problems that affect them. It provides a discussion on the composition and corrosive nature of white water. The article also presents a description of specific corrosion mechanisms. It addresses the corrosion and chemical recovery associated with kraft pulping liquors.

You do not currently have access to this content.
Don't already have an account? Register

Harry Dykstra, 2006. "Corrosion in the Pulp and Paper Industry", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal