Book Chapter

Corrosion in Microelectronics

By
Jianhai Qiu
Jianhai Qiu
Nanyang Technological University
,
Singapore
Search for other works by this author on:
Published:
2006
Page range:
613 - 622
Publication history
October 03, 2006

Abstract

This article discusses the influence of the materials, design, package type, and environment on corrosion in microelectronics. It describes the common sources and mechanisms of corrosion in microelectronics, including anodic, cathodic, and electrolytic reactions resulting in uniform corrosion, galvanic corrosion, pitting corrosion, creep corrosion, dendrite growth, fretting, stress-corrosion cracking, and whisker growth. The article presents effective measures for minimizing the moisture retention in hermetic packages and/or moisture ingress in plastic packages. It concludes with information corrosion tests.

You do not currently have access to this content.
Don't already have an account? Register

Jianhai Qiu, 2006. "Corrosion in Microelectronics", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal