Corrosion of Metal Processing Equipment

By
B. Mishra
B. Mishra
Revising author
Colorado School of Mines
Search for other works by this author on:
Published:
2006
Page range:
1067 - 1075
Publication history
October 16, 2006

Abstract

The high-temperature corrosion processes that are most frequently responsible for the degradation of furnace accessories are oxidation, carburization, decarburization, sulfidation, molten-salt corrosion, and molten-metal corrosion. This article discusses each corrosion process, along with the corrosion behavior of important engineering alloys. It describes the corrosion of plating, anodizing, and parts of pickling equipment such as tanks, wirings and bus bars, racks, anode splines, pumps, and heaters.

You do not currently have access to this content.
Don't already have an account? Register

B. Mishra, 2006. "Corrosion of Metal Processing Equipment", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal