Skip to Main Content
ASM Handbook

Corrosion: Environments and Industries

Edited by
Stephen D. Cramer
Stephen D. Cramer
Search for other works by this author on:
Bernard S. Covino, Jr.
Bernard S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13C
ISBN electronic:
978-1-62708-184-9
Publication date:
2006
Book Chapter

Marine Cathodic Protection

By
Robert H. Heidersbach
Robert H. Heidersbach
Dr. Rust, Inc.
Search for other works by this author on:
James Brandt
James Brandt
Galvotec Corrosion Services
Search for other works by this author on:
David Johnson
David Johnson
Galvotec Corrosion Services
Search for other works by this author on:
John S. Smart, III
John S. Smart, III
Consulting Engineers
Search for other works by this author on:
John S. Smart
John S. Smart
Consulting Engineers
Search for other works by this author on:
Published:
2006
Page range:
73 - 78
Publication history
September 15, 2006

Abstract

Cathodic protection (CP) is an electrochemical means of corrosion control widely used in the marine environment. This article discusses the two types of CP systems, namely, impressed current systems and sacrificial anode (passive) systems. It describes the anode materials used in these systems and CP criteria. The article also discusses the design considerations and procedures involved in the CP of marine pipelines, offshore structures, and ship hulls. It also illustrates the sacrificial anode calculation.

You do not currently have access to this content.
Don't already have an account? Register

Robert H. Heidersbach, James Brandt, David Johnson, John S. Smart, III, John S. Smart, 2006. "Marine Cathodic Protection", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal