Corrosion of Metal Artifacts Displayed in Outdoor Environments

By
L.S. Selwyn
L.S. Selwyn
Canadian Conservation Institute
Search for other works by this author on:
P.R. Roberge
P.R. Roberge
Royal Military College of Canada
Search for other works by this author on:
Published:
2006
Page range:
289 - 305
Publication history
September 26, 2006

Abstract

This article describes the various environmental factors that cause corrosion on metal artifacts. These include water, temperature fluctuations, pollutants, local conditions of acidity or alkalinity, vegetation, and animals. The corrosion processes experienced by five common metals used in outdoor artifacts are discussed. The metals include copper alloys, iron alloys, lead, zinc, and aluminum. The article discusses conservation and preservation strategies for these metals. It also provides a discussion on conservation strategies for gold.

You do not currently have access to this content.
Don't already have an account? Register

L.S. Selwyn, P.R. Roberge, 2006. "Corrosion of Metal Artifacts Displayed in Outdoor Environments", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal