Skip to Main Content
ASM Handbook

Corrosion: Environments and Industries

Edited by
Stephen D. Cramer
Stephen D. Cramer
Search for other works by this author on:
Bernard S. Covino, Jr.
Bernard S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13C
ISBN electronic:
978-1-62708-184-9
Publication date:
2006
Book Chapter

Corrosion in High-Temperature Environments

By
George Y. Lai
George Y. Lai
Consultant
Search for other works by this author on:
Published:
2006
Page range:
754 - 761
Publication history
October 11, 2006

Abstract

Understanding the high-temperature corrosion behavior of alloys is an important step toward the selection of appropriate alloys for process equipment. This article briefly describes the high-temperature corrosion modes that are frequently encountered in the chemical process industry. These modes include oxidation, carburization, metal dusting, nitridation, halogen corrosion, and sulfidation.

You do not currently have access to this content.
Don't already have an account? Register

George Y. Lai, 2006. "Corrosion in High-Temperature Environments", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal