Cathodic Protection of Pipe-Type Power Transmission Cables

By
Adrian Santini
Adrian Santini
Con Edison of New York
Search for other works by this author on:
Published:
2006
Page range:
122 - 125
Publication history
September 19, 2006

Abstract

This article provides a detailed discussion on the various devices by which cathodic protection (CP) can be applied to pipe-type power transmission cables. These devices include the resistor rectifier, isolator-surge protector, polarization cells, and field rectifiers. The article describes the interference created by stray currents on CP and associated remedial actions.

You do not currently have access to this content.
Don't already have an account? Register

Adrian Santini, 2006. "Cathodic Protection of Pipe-Type Power Transmission Cables", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal