Skip to Main Content
ASM Handbook

Corrosion: Environments and Industries

Edited by
Stephen D. Cramer
Stephen D. Cramer
Search for other works by this author on:
Bernard S. Covino, Jr.
Bernard S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13C
ISBN electronic:
978-1-62708-184-9
Publication date:
2006
Book Chapter

Stray Currents in Underground Corrosion

By
W. Brian Holtsbaum
W. Brian Holtsbaum
CC Technologies Canada Ltd.
Search for other works by this author on:
Published:
2006
Page range:
107 - 114
Publication history
September 18, 2006

Abstract

Stray current can be defined as a current in structures that are underground or immersed in an electrolyte that most often accelerate corrosion on a structure where a positive current leaves the structure to enter the earth or an electrolyte. This article provides a description of the principles of stray current and a discussion on the major types of stray current and their properties and prediction methods. It discusses the consequences of stray current and describes the interference tests used for mapping the path of the stray currents. The article also highlights the methods of mitigating the source of stray current.

You do not currently have access to this content.
Don't already have an account? Register

W. Brian Holtsbaum, 2006. "Stray Currents in Underground Corrosion", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal