Corrosion by Ammonia

By
Michael Davies
Michael Davies
CARIAD Consultants
Search for other works by this author on:
Published:
2006
Page range:
727 - 735
Publication history
October 10, 2006

Abstract

Ammonia and ammonium hydroxide are not particularly corrosive in themselves, but corrosion problems can arise with specific materials, particularly when contaminants are present. This article discusses the corrosion resistance of materials used for the manufacture, handling, and storage of ammonia. These materials include aluminum alloys, iron and steel, stainless steels, nickel and its alloys, copper and its alloys, titanium and its alloys, zirconium and its alloys, niobium, tantalum, and nonmetallic materials.

You do not currently have access to this content.
Don't already have an account? Register

Michael Davies, 2006. "Corrosion by Ammonia", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.