Skip to Main Content
ASM Handbook

Corrosion: Environments and Industries

Edited by
Stephen D. Cramer
Stephen D. Cramer
Search for other works by this author on:
Bernard S. Covino, Jr.
Bernard S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13C
ISBN electronic:
978-1-62708-184-9
Publication date:
2006
Book Chapter

High-Temperature Corrosion in Military Systems

By
David A. Shifler
David A. Shifler
Naval Surface Warfare Center, Carderock Division
Search for other works by this author on:
Published:
2006
Page range:
156 - 170
Publication history
September 20, 2006

Abstract

High-temperature exposure of materials occurs in many applications such as power plants (coal, oil, natural gas, and nuclear), land-based gas turbine and diesel engines, gas turbine engines for aircraft, marine gas turbine engines for shipboard use, waste incineration, high-temperature fuel cells, and missile components. This article discusses high-temperature corrosion in boilers, diesel engines, gas turbines, and waste incinerators. Boilers are affected by stress rupture failures, waterside corrosion failures, fireside corrosion failures, and environmental cracking failures. Contamination of combustion fuel in diesel engines can cause high-temperature corrosion. Gas turbine engines are affected by hot corrosion. Refractory-lined incinerators and alloy-lined incinerators are discussed. The article provides case studies for each component failure.

You do not currently have access to this content.
Don't already have an account? Register

David A. Shifler, 2006. "High-Temperature Corrosion in Military Systems", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal