Corrosion of Metal Artifacts in Buried Environments

By
Lyndsie S. Selwyn
Lyndsie S. Selwyn
Canadian Conservation Institute
Search for other works by this author on:
Published:
2006
Page range:
306 - 322
Publication history
September 26, 2006

Abstract

The corrosion processes of metals during burial are affected by environmental pollutants, other archaeological material, geography, microorganisms in the soil, vegetation, land use, soil chemistry, soil physical properties, and the presence or absence of water and air. This article discusses key environmental variables that affect the corrosion of buried metal artifacts. These include water (including dissolved salts and gases), sulfate-reducing bacteria, pH (acidity), and potential (oxidizing or reducing capacity). The article contains a table that lists some corrosion products identified on archaeological tin and pewter, lead, iron alloys, silver alloys, and copper alloys. It also discusses the corrosion problems after excavation and the techniques followed by archaeological department for conserving the metal artifacts.

You do not currently have access to this content.
Don't already have an account? Register

Lyndsie S. Selwyn, 2006. "Corrosion of Metal Artifacts in Buried Environments", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal