Corrosion in the Mining and Metal Processing Industries

Published:
2006

Abstract

The high-temperature corrosion processes that are most frequently responsible for the degradation of furnace accessories are oxidation, carburization, decarburization, sulfidation, molten-salt corrosion, and molten-metal corrosion. This article discusses each corrosion process, along with the corrosion behavior of important engineering alloys. It describes the corrosion of plating, anodizing, and parts of pickling equipment such as tanks, wirings and bus bars, racks, anode splines, pumps, and heaters.

Abstract

This article describes the corrosion of principal parts of mining equipment such as mine shafts, wire rope, rock bolts, and pump and piping systems. It discusses the diagnosis and prevention of various types of corrosion including uniform corrosion, pitting corrosion, crevice corrosion, erosion-corrosion, and intergranular corrosion. The article explains the corrosion in tanks, reactor vessels, cyclic loading machinery, and pressure leaching equipment.

You do not currently have access to this content.
Don't already have an account? Register

2006. "Corrosion in the Mining and Metal Processing Industries", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal