Material Issues in the Pharmaceutical Industry

By
Paul K. Whitcraft
Paul K. Whitcraft
Rolled Alloys
Search for other works by this author on:
Published:
2006
Page range:
810 - 812
Publication history
October 11, 2006

Abstract

This article discusses the corrosion characteristics of superaustenitic stainless and duplex stainless steels, which are used in pharmaceutical industry. It describes passivation treatments and the electropolishing of stainless steels. The article informs that electropolishing is not a passivation treatment, although the proper execution of the process will result in a passive surface. The article concludes with a discussion on roughing, which is a phenomenon of particular interest to the pharmaceutical industry.

You do not currently have access to this content.
Don't already have an account? Register

Paul K. Whitcraft, 2006. "Material Issues in the Pharmaceutical Industry", Corrosion: Environments and Industries, S.D. Cramer, B.S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal