Inspection, Data Collection, and Management

By
Sam McFarland
Sam McFarland
Lloyd's Register
Search for other works by this author on:
Published:
2006
Page range:
1037 - 1053
Publication history
August 12, 2006

Abstract

This article focuses on the aspects associated with inspection related to pressure vessels and pipework. These aspects include inspection policy, inspection planning and procedures, inspection strategy, inspection methodology, preparation for inspection, invasive inspection, internal visual inspection, and non-invasive inspection. Inspection execution, risk-based inspection, competence assurance of inspection personnel, inspection coverage, inspection periodicity, inspection anomaly criteria, assessment of fitness, and reporting requirements, are also discussed. The article addresses the data acquisition, reporting and trending, and review and audit for the inspection. It reviews inspection techniques, including visual inspection, ultrasonic inspection, and radiographic inspection.

You do not currently have access to this content.
Don't already have an account? Register

Sam McFarland, 2006. "Inspection, Data Collection, and Management", Corrosion: Environments and Industries, S.D. Cramer, B.S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal