Corrosion of Aluminum Components in the Automotive Industry

By
Greg Courval
Greg Courval
Alcan International Limited
Search for other works by this author on:
Published:
2006
Page range:
545 - 547
Publication history
October 03, 2006

Abstract

This article provides an overview of the principle forms of corrosion that can occur on automotive aluminum components and offers general guidelines on how best to avoid these situations. It discusses the most common forms of aluminum corrosion such as stress-induced corrosion, cosmetic corrosion, crevice corrosion, and galvanic corrosion.

You do not currently have access to this content.
Don't already have an account? Register

Greg Courval, 2006. "Corrosion of Aluminum Components in the Automotive Industry", Corrosion: Environments and Industries, S.D. Cramer, B.S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal