Skip to Main Content
ASM Handbook

Corrosion: Environments and Industries

Edited by
S.D. Cramer
S.D. Cramer
Search for other works by this author on:
B.S. Covino, Jr.
B.S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13C
ISBN electronic:
978-1-62708-184-9
Publication date:
2006
Book Chapter

Corrosion by Phosphoric Acid

By
Ralph (Bud) W. Ross, Jr.
Ralph (Bud) W. Ross, Jr.
Consultant
Search for other works by this author on:
Published:
2006
Page range:
736 - 741
Publication history
October 16, 2006

Abstract

Phosphoric acid is less corrosive than sulfuric and hydrochloric acids. This article discusses the corrosion rates of metal alloys in phosphoric acid, including aluminum, carbon steel and cast irons, stainless steels, nickel-rich G-type alloys, copper and copper alloys, nickel alloys, lead, titanium alloys, and zirconium alloys. Nonmetallic materials may be chemically attacked in some corrosive environments, which can result in swelling, hardening, or softening phenomena; extraction of ingredients; chemical conversion of the nonmetallic constituents; cross-linking oxidation; and/or substitution reactions. The article also describes the corrosion resistance of nonmetallic materials such as rubber and elastomeric materials, plastics, carbon and graphite, and ceramic materials.

You do not currently have access to this content.
Don't already have an account? Register

Ralph (Bud) W. Ross, Jr., 2006. "Corrosion by Phosphoric Acid", Corrosion: Environments and Industries, S.D. Cramer, B.S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal