Book Chapter

Corrosion in Service Water Distribution Systems

By
K. Anthony Selby
K. Anthony Selby
Water Technology Consultants™, Inc.
Search for other works by this author on:
Published:
2006
Page range:
12 - 14
Publication history
September 14, 2006

Abstract

This article describes the corrosion mechanisms, challenges, and control in service water distribution systems. It provides a discussion on typical designs and water qualities for the service water distribution systems used in fossil-fueled and nuclear power plants. The article also describes techniques for controlling corrosion in service water systems.

You do not currently have access to this content.
Don't already have an account? Register

K. Anthony Selby, 2006. "Corrosion in Service Water Distribution Systems", Corrosion: Environments and Industries, S.D. Cramer, B.S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal