Introduction to Corrosion in Specific Environments

By
Stephen D. Cramer
Stephen D. Cramer
National Energy Technology Laboratory, U.S. Department of Energy
Search for other works by this author on:
Published:
2006
Page range:
5 - 7
Publication history
September 14, 2006

Abstract

This article describes the various environments affecting corrosion performance, corrosion protection, and corrosion control. These include freshwater environments, marine environments, and underground environments. The article provides information on corrosion in military environments and specialized environments, representing less-well-known environments with more limited applications.

You do not currently have access to this content.
Don't already have an account? Register

Stephen D. Cramer, 2006. "Introduction to Corrosion in Specific Environments", Corrosion: Environments and Industries, S.D. Cramer, B.S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal