Abstract

The primary fossil fuels are generally defined as coal, oil, natural gas, tar sands, and shale oil. This article discusses the characteristics and the types of fuels used in fossil and fuel industries. It describes the energy conversion in fuels and outlines the efficiency of a heat engine with the help of the Carnot equation.

Abstract

This article focuses on high-temperature corrosion in synthetic gas (syngas) coolers. Extensive laboratory corrosion studies on both model and commercial alloys are summarized. The article describes the material selection criteria for long-term performance of materials in service. It provides information on the fuels with chlorine contents used in gasification plants.

You do not currently have access to this content.
Don't already have an account? Register

2006. "Corrosion in Fossil and Alternative Fuel Industries", Corrosion: Environments and Industries, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal