Corrosion in Military Environments

Published:
2006

Abstract

This article reviews corrosion problems in the U.S. Department of Defense (DoD) and discusses management and maintenance aspects of the practices that address the cost and readiness. It describes the plans to institute corrosion prevention and control strategies under DoD directives in engineering design, material selection, and fabrication processes for new acquisitions. The article also presents long-term strategy to reduce the cost of corrosion control.

Abstract

This article provides a perspective on United States (U.S.) Department of Defense (DOD) specifications, standards, handbooks, and related documents, as well as their role in corrosion prevention and control activities in the U.S. military.

You do not currently have access to this content.
Don't already have an account? Register

2006. "Corrosion in Military Environments", Corrosion: Environments and Industries, S.D. Cramer, B.S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal