Overpotential

Published:
2005
Page range:
663 - 664
Publication history
April 17, 2006

Abstract

Overpotential is the current-producing potential difference between a nonequilibrium electrode potential and its corresponding equilibrium value for an electrode reaction. This article provides information on overpotential of an electrode reaction. It contains a table that lists overpotential values based on the electrode reaction.

You do not currently have access to this content.
Don't already have an account? Register

2005. "Overpotential", Corrosion: Materials, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal