Corrosion of Cemented Carbides

Published:
2005
Page range:
513 - 525
Publication history
April 15, 2006

Abstract

Cemented carbides are extremely important in corrosion conditions in which high hardness, wear resistance, or abrasion resistance is required. This article describes the effect of binder composition and carbide addition on corrosion behavior of cemented carbides. It lists the examples of their uses in corrosion applications. The article provides information on the selection of cemented carbides for corrosion applications and tabulates the corrosion resistance of cemented carbides in various media. It expounds the oxidation resistance of cemented carbides and presents some tips to improve the properties of tungsten carbide cutting tools. The article also details the coating materials and coating processes of cemented carbides.

You do not currently have access to this content.
Don't already have an account? Register

2005. "Corrosion of Cemented Carbides", Corrosion: Materials, Stephen D. Cramer, Bernard S. Covino, Jr.