Skip to Main Content
ASM Handbook

Corrosion: Materials

Edited by
Stephen D. Cramer
Stephen D. Cramer
Search for other works by this author on:
;
Bernard S. Covino, Jr.
Bernard S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13B
ISBN electronic:
978-1-62708-183-2
Publication date:
2005
Book Chapter

Corrosion of Electroplated Hard Chromium

By
Allen R. Jones
Allen R. Jones
Atotech
Search for other works by this author on:
Published:
2005
Page range:
434 - 441
Publication history
April 10, 2006

Abstract

This article discusses the corrosion of chromium electrodeposits and the ways for optimizing corrosion resistance. It describes processing steps and conditions for hard chromium plating. The steps include pretreatment, electroplating, and posttreatment. The article also provides information on duplex coatings and applications of chromium electrodeposits.

You do not currently have access to this content.
Don't already have an account? Register

Allen R. Jones, 2005. "Corrosion of Electroplated Hard Chromium", Corrosion: Materials, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal