Book Chapter

Corrosion of Metal-Matrix Composites

By
L.H. Hihara
L.H. Hihara
The University of Hawaii at Manoa
Search for other works by this author on:
Published:
2005
Page range:
526 - 542
Publication history
April 12, 2006

Abstract

This article begins with the discussion on the background of metal-matrix composites (MMC) and moves into a broad description of the general parameters affecting the corrosion of MMC. It discusses the primary sources of MMC corrosion that include galvanic corrosion between MMC constituents, chemical degradation of interphases and reinforcements, microstructure-influenced corrosion, and processing-induced corrosion. The article elaborates on the corrosion behavior of specific aluminum, magnesium, titanium, copper, stainless steel, lead, depleted uranium, and zinc MMCs systems. It concludes with a description on the corrosion control of MMCs using protective coatings and inhibitors.

You do not currently have access to this content.
Don't already have an account? Register

L.H. Hihara, 2005. "Corrosion of Metal-Matrix Composites", Corrosion: Materials, Stephen D. Cramer, Bernard S. Covino, Jr.