Abstract

This article is a guide that rates the compatibility of dissimilar structural materials joined together for service in seawater, marine atmosphere, or industrial atmosphere. It contains a table that indicates the material code and most generally effective surface treatment typically used to reduce corrosion of bare metal.

You do not currently have access to this content.
Don't already have an account? Register

2005. "Compatibility Guide", Corrosion: Materials, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal