Skip to Main Content
ASM Handbook

Corrosion: Materials

Edited by
Stephen D. Cramer
Stephen D. Cramer
Search for other works by this author on:
Bernard S. Covino, Jr.
Bernard S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13B
ISBN electronic:
978-1-62708-183-2
Publication date:
2005
Book Chapter

Corrosion of Zinc and Zinc Alloys

By
X. Gregory Zhang
X. Gregory Zhang
Teck Cominco Metals Ltd.
Search for other works by this author on:
Published:
2005
Page range:
402 - 417
Publication history
April 12, 2006

Abstract

Zinc is one of the most used metals, ranking fourth in worldwide production and consumption behind iron, aluminum, and copper. This article commences with an overview of the applications of zinc that can be divided into six categories: coatings, casting alloys, alloying element in brass and other alloys, wrought zinc alloys, zinc oxide, and zinc chemicals. It discusses the corrosion and electrochemical behavior of zinc and its alloys in various environments, particularly in atmospheres in which they are most widely used. The article tabulates the corrosion rates of zinc and zinc coatings immersed in various types of waters, in different solutions in the neutral pH range, and in soils at different geographic locations in the United States. It concludes with information on the forms of corrosion encountered in zinc coatings, including galvanic corrosion, pitting corrosion, and intergranular corrosion.

You do not currently have access to this content.
Don't already have an account? Register

X. Gregory Zhang, 2005. "Corrosion of Zinc and Zinc Alloys", Corrosion: Materials, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal