Degradation of Protective Coatings

By
Kenneth B. Tator
Kenneth B. Tator
KTA-Tator, Inc.
Search for other works by this author on:
Published:
2005
Page range:
589 - 599
Publication history
April 10, 2006

Abstract

Paints and protective coatings are the most common means of protecting materials from deterioration. This article focuses on coating degradation resulting from the environmental interaction with the coatings. The major environmental influences that result in coating degradation include energy (solar radiation, heat and temperature variation, and nuclear radiation), permeation (moisture, solvent retention, chemical, and oxygen), stress (drying and curing, vibration, and impact and abrasion), and biological influences (microbiological and macrobiological).

You do not currently have access to this content.
Don't already have an account? Register

Kenneth B. Tator, 2005. "Degradation of Protective Coatings", Corrosion: Materials, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal