Corrosion of Cast Stainless Steels
By
Malcolm Blair
Malcolm Blair
Revising author
Steel Founders′ Society of America
Search for other works by this author on:
Published:
2005
Page range:
78 - 87
Publication history
April 05, 2006
Abstract
Cast stainless steels are usually specified on the basis of composition by using the alloy designation system established by the Alloy Casting Institute. This article discusses the corrosion behavior of heat-resistant alloys due to oxidation, sulfidation, and carburization. It describes the influence of the metallurgy of corrosion-resistant stainless steels on general corrosion, intergranular corrosion, localized corrosion, corrosion fatigue, and stress corrosion.
You do not currently have access to this content.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InMalcolm Blair, 2005. "Corrosion of Cast Stainless Steels", Corrosion: Materials, Stephen D. Cramer, Bernard S. Covino, Jr.
Download citation file:
×
Advertisement
Mager
Mager Scientific is your exclusive source for Qness hardness testing equipment in the United States.