Skip to Main Content
ASM Handbook

Corrosion: Materials

Edited by
Stephen D. Cramer
Stephen D. Cramer
Search for other works by this author on:
Bernard S. Covino, Jr.
Bernard S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13B
ISBN electronic:
978-1-62708-183-2
Publication date:
2005
Book Chapter

Corrosion of Organic Coated Steels

By
Hiroyuki Tanabe
Hiroyuki Tanabe
Revising author
Dai Nippon Toryo Company
Search for other works by this author on:
Published:
2005
Page range:
40 - 42
Publication history
April 04, 2006

Abstract

This article describes the paint systems generally used to protect steel structures, steel sheet, and bridges from corrosion, and how they deter corrosion. It provides a discussion on the basic design criteria of steel structures for corrosion protection. The article also explains the differences between prepaint and postpaint, and the steps involved in prepaint processing of steel. It presents the selection guideline for paint system evaluation. The advantages of corrosion protection are also discussed.

You do not currently have access to this content.
Don't already have an account? Register

Hiroyuki Tanabe, 2005. "Corrosion of Organic Coated Steels", Corrosion: Materials, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal