Skip to Main Content
ASM Handbook

Corrosion: Materials

Edited by
Stephen D. Cramer
Stephen D. Cramer
Search for other works by this author on:
Bernard S. Covino, Jr.
Bernard S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13B
ISBN electronic:
978-1-62708-183-2
Publication date:
2005
Book Chapter

Thermal Spray Coatings for Corrosion Protection in Atmospheric and Aqueous Environments

By
Seiji Kuroda
Seiji Kuroda
National Institute for Materials Science
Search for other works by this author on:
Andrew Sturgeon
Andrew Sturgeon
TWI, Ltd.
Search for other works by this author on:
Published:
2005
Page range:
422 - 429
Publication history
April 06, 2006

Abstract

This article provides a general technical description of thermal spray coatings used for corrosion protection in atmospheric and aqueous environments. It further discusses two basic coating approaches of corrosion protection, namely, the sacrificial coating of thermal spray aluminum (TSA) and thermal spray zinc (TSZ), and the barrier-type coating of corrosion-resistant materials. The emphasis is on sacrificial coatings. The article describes the steps involved in the application of TSA and TSZ: surface preparation, coating deposition, and postspray treatment. It discusses their field exposure tests and application history. The article also contains helpful information on the dense barrier coatings by high-velocity spraying processes along with their corrosion performance.

You do not currently have access to this content.
Don't already have an account? Register

Seiji Kuroda, Andrew Sturgeon, 2005. "Thermal Spray Coatings for Corrosion Protection in Atmospheric and Aqueous Environments", Corrosion: Materials, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal