Environmental Performance of Rubber Linings

By
Larry DeLashmit
Larry DeLashmit
Polycorp, Ltd.
Search for other works by this author on:
Published:
2005
Page range:
605 - 607
Publication history
April 07, 2006

Abstract

Natural and synthetic rubber linings are used extensively in many industries for their corrosion and/or abrasion resistance. These industries include transportation, chemical processing, water treatment, power, mineral processing, and mining. This article provides information on soft natural rubber, semihard natural rubber, hard natural rubber, neoprene or polychloroprene, chlorobutyl, three-ply linings, nitrile, and ethylene propylene with a diene monomer. Emphasis is placed on advantages, disadvantages, and common uses of each material discussed.

You do not currently have access to this content.
Don't already have an account? Register

Larry DeLashmit, 2005. "Environmental Performance of Rubber Linings", Corrosion: Materials, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal