Pressing and Sintering of Copper Powders

By
Wayne K. Daye
Wayne K. Daye
ACuPowder International/ECKA Granules/SCM Metal Products, Inc.
Search for other works by this author on:
Thomas W. Pelletiers, II
Thomas W. Pelletiers, II
ACuPowder International/ECKA Granules/SCM Metal Products, Inc.
Search for other works by this author on:
Published:
2015
Page range:
555 - 557
Publication history
August 25, 2015

Abstract

Development of the properties of copper powder metallurgy parts is affected by pressing and sintering processes used in the production of components, such as contacts, carbon brushes, and friction materials. This article briefly describes the powder properties of copper and discusses the roles of lubricant and compaction dies in pressing of copper powders. It explains the structural defects that originate during the compaction process of PM parts. The article also provides information on sintering, re-pressing, and re-sintering of copper PM parts.

You do not currently have access to this content.
Don't already have an account? Register

Wayne K. Daye, Thomas W. Pelletiers, II, 2015. "Pressing and Sintering of Copper Powders", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal