Powder Metallurgy Nickel and Nickel Alloys

By
Lou Koehler
Lou Koehler
Koehler Associates
Search for other works by this author on:
Published:
2015
Page range:
673 - 681
Publication history
August 27, 2015

Abstract

This article discusses the methods for producing powder metallurgy (PM) nickel powders, including carbonyl process, hydrometallurgical process, hydrogen reduction process, and atomization process, as well as their applications. It describes three processes for producing nickel alloy powders: water atomization, high-pressure water atomization, and gas atomization. The article also provides information on the applications of PM hot isostatic pressing in the oil and gas industry.

You do not currently have access to this content.
Don't already have an account? Register

Lou Koehler, 2015. "Powder Metallurgy Nickel and Nickel Alloys", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal