Corrosion Resistance of Powder Metallurgy Stainless Steels

By
Prasan K. Samal
Prasan K. Samal
Consultant
Search for other works by this author on:
Published:
2015
Page range:
447 - 457
Publication history
August 24, 2015

Abstract

This article reviews various test methods used for evaluating the corrosion resistance of powder metallurgy stainless steels. These include immersion testing, salt spray testing, and electrochemical testing. The article discusses the factors that affect corrosion resistance of sintered stainless steels: compaction-related factors, sintering-related factors, and effects of alloy composition. Corrosion resistance data for sintered stainless steels is provided.

You do not currently have access to this content.
Don't already have an account? Register

Prasan K. Samal, 2015. "Corrosion Resistance of Powder Metallurgy Stainless Steels", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal