Beryllium and Aluminum-Beryllium Alloys

By
Don H. Hashiguchi
Don H. Hashiguchi
Materion Corporation
Search for other works by this author on:
Mark Svilar
Mark Svilar
Materion Corporation
Search for other works by this author on:
Aaron B. Sayer
Aaron B. Sayer
Materion Corporation
Search for other works by this author on:
Amanda L. Morales
Amanda L. Morales
Materion Corporation
Search for other works by this author on:
Published:
2015
Page range:
757 - 765
Publication history
August 29, 2015

Abstract

This article briefly describes the production of beryllium powder and beryllium/beryllium oxide metal-matrix powder. It discusses fully dense consolidation methods: vacuum hot pressing, hot isostatic pressing, and cold isostatic pressing. Secondary fabrication operations of beryllium and aluminum-beryllium alloys such as extrusion, rolling, welding, joining, and machining are discussed. The article discusses quality control and provides information on the structural, optical, and high-purity grades of beryllium.

You do not currently have access to this content.
Don't already have an account? Register

Don H. Hashiguchi, Mark Svilar, Aaron B. Sayer, Amanda L. Morales, 2015. "Beryllium and Aluminum-Beryllium Alloys", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal