Skip to Main Content
ASM Handbook

Powder Metallurgy

Edited by
P. Samal
P. Samal
Search for other works by this author on:
J. Newkirk
J. Newkirk
Search for other works by this author on:
ASM International
Volume
7
ISBN electronic:
978-1-62708-175-7
Publication date:
2015
Book Chapter

Sintering of Stainless Steels

By
Peter A. dePoutiloff
Peter A. dePoutiloff
SSI Sintered Technologies
Search for other works by this author on:
Prasan K. Samal
Prasan K. Samal
Consultant
Search for other works by this author on:
Published:
2015
Page range:
433 - 439
Publication history
August 24, 2015

Abstract

This article describes the sintering behavior of austenitic, ferritic, and martensitic stainless steels. It presents different sintering schedules that are selected by Metal Powder Industries Federation (MPIF). The article provides information on the equipment and atmospheres used for sintering and the steps involved in the process. It discusses the factors that influence the dimensional changes in sintering, namely, powder-related, compaction-related, and sintering-related factors.

You do not currently have access to this content.
Don't already have an account? Register

Peter A. dePoutiloff, Prasan K. Samal, 2015. "Sintering of Stainless Steels", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal