Manufacture of Stainless Steel Powders

By
Roland T. Warzel, III
Roland T. Warzel, III
North American Höganäs, Inc.
Search for other works by this author on:
Published:
2015
Page range:
421 - 426
Publication history
August 24, 2015

Abstract

This article provides information on the process details that differ from general water atomization of metals as they relate to basic and engineering properties that are specific to stainless steel powders. The discussion focuses on the compacting-grade stainless steel powders. The process details include raw materials, melting method, and control of physical and chemical powder characteristics. The article describes the gas atomization of stainless steel powders and processes that are done after water atomization: drying, screening, annealing, and lubricating. It also discusses the two types of quality assurance testing measures for powder metallurgy stainless steels: tests for powder contamination and tests of chemical and physical properties.

You do not currently have access to this content.
Don't already have an account? Register

Roland T. Warzel, III, 2015. "Manufacture of Stainless Steel Powders", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal