Skip to Main Content
ASM Handbook

Powder Metallurgy

Edited by
P. Samal
P. Samal
Search for other works by this author on:
J. Newkirk
J. Newkirk
Search for other works by this author on:
ASM International
Volume
7
ISBN electronic:
978-1-62708-175-7
Publication date:
2015
Book Chapter

Cemented Carbide Quality Control

By
Gary Runyon
Gary Runyon
Kennametal Firth Sterling
Search for other works by this author on:
Binky Sargent
Binky Sargent
Kennametal Inc.
Search for other works by this author on:
Published:
2015
Page range:
729 - 732
Publication history
August 26, 2015

Abstract

Quality control of cemented carbides includes the evaluation of physical and chemical properties of constituent raw material powders, powder blends/formulations, green compacts, and fully dense finished product. This article provides a summary of the underlying principles and size ranges for the American Society for Testing and Materials (ASTM) standard methods of particle sizing and distribution. It presents the methods used to analyze the chemical composition of cemented carbide materials in a tabular form. The article also presents information on microstructural evaluation and physical and mechanical property evaluation of cemented carbides.

You do not currently have access to this content.
Don't already have an account? Register

Gary Runyon, Binky Sargent, 2015. "Cemented Carbide Quality Control", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal