Ferrous Powder Metallurgy Materials[1]

By
W. Brian James
W. Brian James
Revising author
Hoeganaes Corp.
Search for other works by this author on:
Published:
2015
Page range:
295 - 310
Publication history
August 22, 2015

Abstract

This article summarizes the general classification, mechanical properties, and applications of ferrous powder metallurgy (PM) materials for parts production. It discusses four principal ferrous PM alloy types: admixed elemental alloys, diffusion alloys, prealloys, and hybrid alloys. The article reviews the benefits and disadvantages as well as the effect of processing on the properties and material microstructure of these alloys. It contains tables that list the mechanical properties of various iron-copper and copper steels.

You do not currently have access to this content.
Don't already have an account? Register

W. Brian James, 2015. "Ferrous Powder Metallurgy Materials", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal