High-Temperature Sintering of Ferrous Powder Metallurgy Components[1]

By
Roland Warzel, III
Roland Warzel, III
Revising author
North American Höganäs
Search for other works by this author on:
Published:
2015
Page range:
331 - 336
Publication history
August 22, 2015

Abstract

High-temperature sintering of ferrous components continues to be important in the powder metallurgy (PM) industry. Improvements in both production rates and properties are possible as sintering temperatures increase above 1120 deg C. This article provides an overview of the different various stages of the sintering process and the physical, chemical, and metallurgical phenomena occur within the mass of metal powder particles. It discusses the four advantages of high-temperature sintering of various ferrous PM materials: improved mechanical properties, improved physical properties, development of liquid phase, and ability to sinter active elements in alloy steels. The article also provides information on three sources of process control requirements, namely, the powder blend, green density, and sintering conditions.

You do not currently have access to this content.
Don't already have an account? Register

Roland Warzel, III, 2015. "High-Temperature Sintering of Ferrous Powder Metallurgy Components", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal