Book Chapter

Introduction to Powder Metallurgy Stainless Steels

By
Prasan K. Samal
Prasan K. Samal
Consultant
Search for other works by this author on:
Published:
2015
Page range:
413 - 414
Publication history
August 22, 2015

Abstract

Stainless steels are highly alloyed materials in comparison to most other popular powder metallurgy (PM) materials, such as low-alloy steels, copper alloys, and aluminum alloys. This article provides an overview of the history of PM stainless steels.

You do not currently have access to this content.
Don't already have an account? Register

Prasan K. Samal, 2015. "Introduction to Powder Metallurgy Stainless Steels", Powder Metallurgy, P. Samal, J. Newkirk