Microstructure of Powder Metallurgy Tool Steels

By
Paul Beiss
Paul Beiss
RWTH Aachen University
Search for other works by this author on:
Published:
2015
Page range:
533 - 535
Publication history
August 25, 2015

Abstract

The microstructure in the longitudinal direction of conventional high-alloy tool steels (HATS) depends very much on the degree of hot working. Comparing different processes, the highest processing temperature proves to be decisive for coarseness of the microstructure. This article provides a discussion on the microstructure of conventional HATS and hot isostatically pressed high-speed steel. The effects of the processing in cold worked HATS are illustrated.

You do not currently have access to this content.
Don't already have an account? Register

Paul Beiss, 2015. "Microstructure of Powder Metallurgy Tool Steels", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal